Indium oxide lattice expands upon doping with tin
Lattice parameter is 10.117 Å in In2O3.
Lattice parameter increases to 10.125 Å
as tin is added up to 6% Sn doping.
Nadaud et al.
J. Solid State Chem.
135, 1988, 140